SnowPod metal 3D printing material roadmap

Material Roadmap. Tested Data.

Explore the SnowPod material roadmap and see how we test surface finish, tensile properties, and nickel release.

SnowPod Material Roadmap

Six material families. Three stages of development.

01

Kickstart & Support

Primary launch + confirmed support

316L
316LPrimary launch
17-4PH
17-4PHSupport confirmed
02

Testing & Development

Release subject to validation

CoCr
CoCrCobalt-chromium alloys
CuCrZr
CuCrZrCopper-chromium-zirconium
03

Future Candidates

Possible development · Not guaranteed

304
304Austenitic stainless steel
420
420Martensitic stainless steel
CuZn alloys
CuZn alloysBrass
CuSn10
CuSn10Tin bronze
Alloy 718
Alloy 718Nickel-based superalloy
H13
H13Hot-work tool steel
Pure silver
Pure silverAg
Sterling silver
Sterling silver925 silver

Future candidates are exploratory. Development and release are not guaranteed.

316L Surface Roughness

Printed on SnowPod. As-built samples.

0° Top surface (Ra)

2.79µm

0° Top surface (Ra)

90° Side surface (Ra)

6.5µm

90° Side surface (Ra)

45° Downward-facing surface (Ra)

9.01µm

45° Downward-facing surface (Ra)

Test data only. As-built condition. Test standards: GB/T 3505 (ISO 4287, IDT) and GB/T 10610 (ISO 4288, IDT). Based on sample testing conducted at SnowX's laboratory.

Material Test Data

Select a material to view its tensile properties and chemical composition.

316L Performance at a Glance

Conceptual illustration of 316L grain structure
Conceptual illustration of grain structure. Not an actual micrograph.
Ultimate Tensile StrengthUltra-high strength grade
729 MPaXY orientation
618 MPaZ orientation
Yield StrengthUltra-high strength grade
617 MPaXY orientation
518 MPaZ orientation
Elongation at BreakExcellent Ductility
32.5 %XY orientation
32.5 %Z orientation
Vickers HardnessWear-Resistant
≥ 220 HV0.5
Nickel ReleaseBio-Safe
Not detected

Note: All data are based on as-built samples, precisely measured by an authoritative third-party testing organization in accordance with the latest Chinese national standards, including GB/T 4340.1-2024.

Download Datasheet

Chemical Composition

ElementCSPCrSiMnMoNiFe
Specified (wt.%)≤0.03≤0.03≤0.04516–18≤1≤22–310–14Bal.
Measured (wt.%)0.0150.010.03417.30.551.022.210.6Bal.

Tensile Properties

Tensile testing was performed on as-built specimens in accordance with GB/T 228.1 (ISO 6892-1, MOD).

316L tensile test sample printed on SnowPod
Tensile Properties
TransverseXY orientation
LongitudinalZ orientation
Ultimate Tensile Strength729 MPa618 MPa
Yield Strength617 MPa518 MPa
Elongation32.5 %32.5 %
Reduction of Area52 %52 %
Elastic Modulus184.4 GPa163.2 GPa

Test data only. Based on sample testing conducted at SnowX's laboratory.

Nickel Release

The samples were immersed in artificial sweat solution for 168 hours (7 days), after which nickel release was measured by ICP-OES.

316L nickel release test sample
Nickel release sample A, as-built
Sample AAs-built
Nickel release sample B, polished
Sample BPolished
Nickel release sample C, acid-pickled and polished
Sample CAcid-pickled & polished
Test SampleABC
Sample Area Tested (cm²)3029.529
Artificial Sweat Solution (mL)505050
Released Nickel
Not detectedBelow the method detection limit of 0.05 µg/cm²/week
Test Result
Passed
Passed
Passed

About the EN 1811 test

EN 1811 measures nickel release from products intended for prolonged skin contact. The samples were immersed in artificial sweat solution for 168 hours (7 days), then analyzed by ICP-OES.

Test data only. Results shown for the three tested 316L samples.

Sign up for releases and product updates